Products

+
  • 石膏细密发泡技术 拷贝.jpg

Gypsum fine-pore foaming technology equipment

Nantong Fleck Fluid Equipment CO., LTD. is a specialized equipment technology manufacturer engaged in the research and development, design, production and sales of wet shear crushing, dispersion emulsification, crushing and grinding, mixing and homogenization, garbage disposal and other equipment. Currently, it has 1 new technology research and development building, 1 graduate practice building, 1 new product project research and development team, and 2 "production, learning and research" cooperation units in universities.

Key words: shear pump | wet mill | rice refiner

Classification:

New technologies and new products

  • Product Description
  • The gypsum slurry foaming technology equipment (fine-cell foamer) uses a foaming agent to generate a large number of uniformly distributed, closed pores within the gypsum slurry, significantly reducing the material’s density and enhancing its thermal insulation performance while maintaining a certain level of mechanical strength. Moreover, the bubbles produced by the fine-cell foamer equipment are approximately 0.5 mm in size and are extremely evenly dispersed throughout the gypsum slurry.

    Product Features

    Technical Principle

    Gypsum slurry foaming technology is mainly divided into two methods: physical foaming and chemical foaming. In physical foaming, a foaming agent is introduced into a foaming device to generate fine, dense bubbles, which are then uniformly mixed with the gypsum slurry. The foaming agent typically consists of an anionic surfactant (such as sodium dodecyl sulfate) combined with a foam-stabilizing agent (such as triterpene saponins). By leveraging the surfactant’s ability to reduce the surface tension of the liquid phase, stable air bubbles are formed. These bubbles create a uniformly distributed pore structure within the gypsum slurry. As the gypsum hydration reaction proceeds, the slurry gradually hardens, and the bubbles become permanently entrapped within the gypsum matrix.

    Chemical foaming: This process involves the use of a foaming agent that undergoes a chemical reaction within the gypsum-based slurry, generating gas that causes the slurry to expand and form a porous structure. Commonly used chemical foaming agents include inorganic foaming agents such as sodium bicarbonate and ammonium carbonate, as well as organic foaming agents like azodicarbonamide and p-toluenesulfonhydrazide. Under specific conditions, these foaming agents decompose to produce gases such as carbon dioxide, thereby forming bubbles within the gypsum slurry.

    Main process flow

    1. Raw Material Preparation: Mix building gypsum powder, water, a set-retarding agent, and a water-reducing agent according to specified proportions to prepare the gypsum slurry. The set-retarding agent (such as gelatin) can delay the setting time of gypsum, ensuring sufficient working time.

    2. Preparation of the foaming agent: The foaming agent is mixed with water according to a specified ratio and then processed through a foaming device to produce stable foam. The foaming agent is typically formulated from anionic surfactants and foam-stabilizing agents, with a foaming multiple ranging from 18 to 40 times and a foam stability lasting over 4 hours.

    3. Mixing: Thoroughly mix the prepared foam with the gypsum slurry, maintaining a stirring speed of 100–200 r/min for 2–3 minutes to ensure that the foam is evenly dispersed throughout the slurry.

    4. Molding and Curing: Pour the foaming slurry into molds, perform initial curing until the compressive strength reaches at least 2.0 MPa, then demold. Afterward, proceed with natural curing.

    Product Parameters

    Key technical parameters

    • Dosage of foaming agent: Typically 0.2–0.5% of the gypsum dosage, adjustable according to the required product density.

    • Water-to-cement ratio: typically 0.6–0.8:1

    • Retarder dosage: 0.1–0.2 wt%, which can extend the initial setting time from 5 minutes to 31 minutes.

    • Stabilizer dosage: At 0.8 wt%, the foam defoaming rate decreases by 18%, and the bubble structure becomes more uniform.

    • Foaming temperature: 15–25℃, with an optimal range of around 20℃.

    Product Performance Specifications

    The material prepared using gypsum slurry foaming technology has the following characteristics:

    • Density: 300–600 kg/m³, significantly lower than that of conventional gypsum products.

    • Compressive strength: 0.4–2.0 MPa, meeting the requirements for lightweight wall materials.

    • Thermal conductivity: 0.080–0.115 kcal/m·h·℃, with excellent thermal insulation performance.

    • Closed-cell rate: ≥90%; the closed-cell structure effectively enhances thermal insulation performance.

    • Water absorption rate: ≤25%, with excellent waterproof performance.

    Product appearance

图片名称

Note: Our company can tailor solutions based on the characteristics of your material medium:

1. Conduct material testing using production-grade equipment

2. Customize equipment selection according to your material's technical specifications

3. Different materials require distinct internal structures. The following equipment internal diagrams are provided for user reference.

For detailed technical specifications, please contact:

Technical Support: 18962835399 18068155581

Sales Hotline: 18912883100 18921623100

Copyright © Nantong Fleck Fluid Equipment CO., LTD. All rights reserved. Unauthorized reproduction is strictly prohibited.

Related Products


High gravity reactor


The material A in the reaction tank is metered to the premixing reaction device at constant pressure through the circulating pump, and the material B in the metering tank also enters the distributor of the premixing reaction device through the flowmeter to carry out the primary mixing reaction with the material A.

Messages

Security verification
Submission